Thermal Ceramics PM Kaowool Low Temperature Boards
Subcategory: Kaolin
Material Notes: Kaowool PM is manufactured to close tolerances with an excellent surface finish. Kaowool PM has a good thermal conductivity and can easily be die-cut.Features: Excellent thermal conductivity Capability to withstand chemical attack Board capabilities are 48 x 36 x 1/4 to 3" (120 x 90 x 0.625 to 7.5 cm) with the exception of PM Board which can be made 1/8" (3.125 cm) thick Applications: Appliance and heat processing insulation Back up in steel ladle and torpedo cars Backup insulation to dense refractories Combustion chamber construction Expansion joint material Flue and chimney linings Furnace, kiln, and oven hot face linings General molten metal contact Glass coffin walls Glass regenerator insulation Glass tank side, end wall and port neck Glass tank wall and port neck insulation Heat shields High temperature gaskets and seals High mechanical stress areas Kiln furniture Trough linings in contact with aluminumInformation provided by Thermal Ceramics
| Available Properties |
- Density
- Loss On Ignition
- Modulus of Rupture
- Compressive Strength
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|