Thermal Ceramics 17C Kaowool High Temperature Boards
Subcategory: Kaolin
Material Notes: Kaowool 17C is processed using a blend of high purity ceramic fibers, high temperature alumina fibers and binders. This combination produces a product with improved high temperature stability. Kaowool 17C exhibits excellent shrinkage and mechanical strengths after firing for temperatures up to 2900°F (1593°C)..Applications: Appliance and heat processing Backup insulation to dense refractories Bullnose tiles Burner blocks Combustion chamber construction Expansion joint material Flue and chimney linings Furnace components Furnace door linings Furnace, kiln, and oven hot face linings Glass regenerator insulation Heat shields High temperature gaskets and seals Peep door frames and plugs Shapes in ammonia reformersInformation provided by Thermal Ceramics
| Available Properties |
- Density
- Loss On Ignition
- Modulus of Rupture
- Compressive Strength
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|