Thermal Ceramics 2800 RPC Shapes
Material Notes: RPC 2800 is an insulating material produced by blending alumina-silicate fibers and alumina fibers with high purity silica binders. The polycrystalline alumina fibers form a matrix within the material, and give it high temperature capability. The high temperature capability is further enhanced by employing ammonia stabilized colloidal silica rather than sodium stabilized product. At elevated temperatures, residual sodium acts as a flux and reduces the refractories maximum use temperature.Features: No organic binders Complex shape capability Low thermal conductivity and minimal heat storage High resistance to thermal shock and spalling Low shrinkage Light weight Applications: Bullnose tiles Burner blocks Combustion chamber construction Diffusion furnaces Flue and exhaust stack liners Furnace components General molten metal contact Peep door frames and plugs Heat shields High temperature gaskets and seals Hot tops for super alloy casting Molten aluminum contact Semiconductor processing equipment Shapes for laboratory furnaces Shapes in ammonia reformersInformation provided by Thermal Ceramics
| Available Properties |
- Density
- Loss On Ignition
- Hardness, Shore A
- Modulus of Rupture
- Compressive Strength
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|