Thermal Ceramics RPC™ 2300-W Wet Felt
Material Notes: Wet Felt is a high-alumina, ceramic fiber material made by a vacuum forming process that produces a unique insulating process capable of withstanding 2300°F (1260°C). Bonded with our standard bond, it has virtually unlimited uses. It is shipped wet in sheets, rolled or flat, and sealed in protective plastic bags. Standard sizes are 48 x 36 x 1/8 to 1" (1200 x 900 x 3.125 to 25mm) thick.Features: Non-self sticking and can be joined by air-set mortar Drying time is 24 to 48 hours Maintains wet shape and characteristics of prefired material after drying Random fiber orientation and a tightly knit structure Collodial silica is disbursed uniformly throughout the entire piece and does not drain out Does not require costly dryers, tooling or machining to conform to size requirementsApplications: Wrapping exhaust manifolds in marine engines Wrapping fuel injector nozzles in solid fuel fired kilns Lining combustion duct work in incinerators and boilers
Lining hot tuyers in upcomers of blast furnaces Hand packed to protect the anchor of an element hanger moduleInformation provided by Thermal Ceramics
| Available Properties |
- Hardness, Shore A
- Modulus of Rupture
- Compressive Strength
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|