Thermal Ceramics 100 Ceraboard

 

Material Notes:
Ceraboard is a refractory fibre board supplied in panels of standard thicknesses made from a slurry of refractory fibres and binders which have a low organic content.

Features:

  • High temperature stability
  • Low thermal conductivity
  • Low heat storage
  • Rigidity and high cohesive strength allow machining and cutting
  • Resistant to thermal shock
  • Good erosion resistance
  • Can be used in direct contact with flame
  • Easy application
  • Applications:This versatile board can be used where a rigid, self supporting and insulating product is required which also has good resistance to physical damage.

  • Ceramic industry (klin linings & klin car insulation)
  • Glass industry
  • High temperature expansion joints
  • High temperature insulation
  • Tundish covers
  • Back-up in steel ladle and torpedo caps
  • Back-up to dense refractories
  • High temperature gaskets and seals
  • Combustion chamber construction
  • Flue and chimney linings
  • Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Loss On Ignition
    • Modulus of Rupture
    • Compressive Strength
    • Thermal Conductivity
    • Melting Point
    • Maximum Service Temperature, Air
    • Shrinkage
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。