Thermal Ceramics 100 Ceraboard
Material Notes: Ceraboard is a refractory fibre board supplied in panels of standard thicknesses made from a slurry of refractory fibres and binders which have a low organic content.Features: High temperature stability Low thermal conductivity Low heat storage Rigidity and high cohesive strength allow machining and cutting Resistant to thermal shock Good erosion resistance Can be used in direct contact with flame Easy applicationApplications:This versatile board can be used where a rigid, self supporting and insulating product is required which also has good resistance to physical damage. Ceramic industry (klin linings & klin car insulation) Glass industry High temperature expansion joints High temperature insulation Tundish covers Back-up in steel ladle and torpedo caps Back-up to dense refractories High temperature gaskets and seals Combustion chamber construction Flue and chimney liningsInformation provided by Thermal Ceramics
| Available Properties |
- Density
- Loss On Ignition
- Modulus of Rupture
- Compressive Strength
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|