Thermal Ceramics TE 1400 Board and Shapes Molded Min-K Insulation
Material Notes: Min-K TE 1400 is used in contact with lead telluride thermoelectric devices, and lend support to thermoelectric heat sources. TE 1400 has a fibrous component developed for improved material strength. While TE 1400 can be machined, it does not lend itself to direct molding of intricate shapes.Features: Microporous Low thermal conductivity Compression resistant Machined to customer specification Lightweight OrganicApplications: Aerospace High temperature Thermoelectric devices Instrumentation and analytical equipmentInformation provided by Thermal Ceramics