Thermal Ceramics 2000 Min-K Data Recorder Molded Min-K Insulation
Material Notes: Min-K Data Recorder materials (so named because of their application in protecting Flight Data Recorder and Cockpit Voice Recorder memory chips) are a specific group of materials available in two types: endothermic and non-endothermic. Min-K 2000 is typically supplied in 20 pcf and Min-K 1303 at 35 pcf density are easily molded and/or machined to customer requirements. Molded Min-K insulation has been used successfully in manned spacecraft, aircraft, and similar high-temperature applications where low thermal conductivity plus space and weight savings are a critical consideration.Features: Microporous Low thermal conductivity Compression resistant Machined to customer specifications Lightweight Endothermic protection Organic freeInformation provided by Thermal Ceramics
| Available Properties |
- Transverse Strength
- Compressive Strength
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|