Thermal Ceramics Standard Min-K Insulating Tape

 

Material Notes:
Flexible Min-K insulating tape is constructed of Min-K core material enclosed with heat-resistant fabrics stitched in parallel pattern. Available in a range of widths and thicknesses, the tape provides the many advantages of flexible Min-K blankets, enabling it to achieve maximum insulating effect in minimum space.

Min-K tape has a lower thermal conductivity than the molecular conductivity of still air, as well as significantly reduced conductivity at high attitudes. It is particularly effective in controlling thermal transients and provides high resistance to potential damage from compression and vibration.

Features:

  • Easy to use
  • Flexible
  • Variety of thicknesses and sizes
  • Applications

  • Fuel, oil and hydraulic lines
  • Ducts
  • Compressors and de-icing equipment
  • High temperature tubing and piping systems
  • A variety of hard-to-insulate areas where weight is critical and working space is minimal
  • Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Thermal Conductivity
    • Maximum Service Temperature, Air
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。