Thermal Ceramics K-Shield Felt AG/Min-K Composite

 

Material Notes:
Thermal Ceramics has recently introduced a composite insulation system which combines the high temperature use limits of ceramic fiber felts with the low thermal conductivity benefits of microporous insulation. This material, a composite of Thermal Ceramics K-Shield Felt AG and the Min-K Division`s microporous core, is available in a quilted form. This composite offers several key advantages over either a traditional microporous material, or a quilted fibrous material, while maintaining the low thermal conductivity (shown below) typically seen in microporous products.

The K-Shield Felt AG/Min-K composite is lighter than comparable Min-K materials. The nominal density of K-Shield Felt AG is 6 pcf, resulting in a final core density of 11 pcf for the 16 pcf Min-K and 7 pcf for the 8 pcf Min-K material, while the thermal conductivity stays virtually constant.

Flexible Min-K is consists of a microporous core and an outer textile facing that typically determines the temperature use limit. High temperature cloths (>1200°F) are often very costly but by using the K-Shield Felt AG on the hot face, the additional cost of cloth may be eliminated. Due to the fibrous nature of ½ the thickness of these composites, costly edge binding may be eliminated in some instances.

By employing the K-Shield Felt AG on the Hot Face, the composite can be used at temperatures greater than the standard maximum temperature use limit of the icroporous core.

The acoustic properties of Min-K and the K-Shield Felt AG are complimentary as each material offers good sound absorption characteristics at different frequencies.

Features:

  • Lightweight
  • Lower cost
  • High temperature use limit
  • Good sound absorption at different frequencies
  • Increased flexibility
  • Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Thermal Conductivity
    • Melting Point
    • Maximum Service Temperature, Air
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。