Thermal Ceramics K-Bond (wet, air setting) Mortar

 

Material Notes:
Thermal Ceramics refractory mortars were developed to match Thermal Ceramics dense and insulating firebricks in various thermal, chemical and physical service conditions. Available in wet and dry grades, Thermal Ceramics mortars will provide the convenience you want with the performance you need for practically every high temperature refractory application. K-Bond Mortar has an extra smooth, creamy consistency plus excellent tackiness to brick surfaces.

Features:

  • Matched for use with each Thermal Ceramics firebrick and insulating firebrick
  • Both heat setting and air setting grades are available
  • Temperature use limits range from 2850°F to 3200°F
  • Information provided by Thermal Ceramics

    Available Properties
    • Maximum Service Temperature, Air
    • Shelf Life
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。