Thermal Ceramics 3000 Kaowool Paper
Material Notes: Kaowool Flex-Wrap is produced from a blend of Kaowool high purity ceramic fibers and organic binders in a unique paper making process. Due to its low organic binder content, offgassing is at a minimum. This specialty paper is noted for its excellent flexibility, outstanding handling characteristics, and high insulating value at high temperatures. Features: High alumina, fiber index and purityOutstanding high temperature stability Thin, flexible, high temperature insulation Easily die-cut to form complex shapes for high temperature gasketing Conforms easily to complex shapes Excellent high temperature parting agentExcellent high temperature backup and expansion joint material Applications: High temperature gaskets and seals Refractory back-up insulation Appliance insulation Separating media for heat treating metals High temperature filtration High temperature expansion joint packing Glassware separating media Parting agent for brazing operations Hot face and backup lining for lab furnaces Aluminum distributor pan lining Super alloy ingot mold lining and hot tapes.Information provided by Thermal Ceramics
| Available Properties |
- Density
- Loss On Ignition
- Tensile Strength, Ultimate
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Other Element Content
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|