Thermal Ceramics LS K-Shield Felt

 

Material Notes:
K-Shield Felt products are produced from premium, cleaned Kaowool high-purity fibers and a special thermosetting binder system in a unique paper-making process. The cleaning process dramatically improves the thermal conductivity, insulating value, and vibration resistance of the felt, while also making it an ideal product for die-cutting, fabrication, and handling. K-Shield Felts are both compressible and resilient, while exhibiting excellent flexibility and handling strengths. The special binder system eliminates smoke problems and allows for minimal off-gassing. Due to their unique semi-rigid yet flexible form, K-Shield Felts offer some special properties in comparison to traditional blankets and papers.

The standard K-Shield Felt, K-Shield Felt LS, and K-Shield Felt AG are premium, low-shot products produced from cleaned high-purity ceramic fibers. The K-Shield Felt LS is a very clean, lower-shot product developed for those very demanding applications. These products have very low thermal conductivites and exhibit excellent vibration resistance.

The K-Shield Felt AG is designed specifically for aerospace insulation applications and is approved for both the BMS9-19 and AMS 3680-Rev. C specifications. These approvals include meeting specific tests related to optimum performance in aerospace insulation applications.

Features:

  • Extremely low thermal conductivity and heat storage
  • Excellent flexibility with good handling strength for fabrication and die-cutting
  • High temperature stability
  • Low organic binder content with minimal off-gassing
  • Low shot (unfiberized material) content
  • Lightweight, yet resilient
  • Continuous use limit of 2300°F (1260°C)
  • Applications:

  • Automotive heat shields and muffler insulation
  • Aerospace insulation
  • High-temperature gasketing
  • Commercial and domestic appliance insulation
  • Expansion joints
  • Parting agent in heat treating and metal working
  • Glassware separator
  • Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Loss On Ignition
    • Tensile Strength, Ultimate
    • Thermal Conductivity
    • Melting Point
    • Maximum Service Temperature, Air
    • Other Element Content
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。