Thermal Ceramics Therm-O-Flake Coating

 

Material Notes:
Therm-O-Flake Coating and Therm-O-Flake Coating-M are lightweight, “fine grained”, gun-applied insulation. They both have an effective temperature range up to 1800°F (982°C). Highly efficient insulations, these coatings are used extensively to reduce radiation loss and air infiltration as well as conserve heat. Therm-O-Flake Coating or Therm-O-Flake Coating-M may be applied to hot or cold surfaces on primary and secondary regenerator walls of glass tanks, reverberatory furnaces, bulkheads, end walls, side walls and arches. They are both particularly effective when used as a sealant over older firebrick walls, bulkheads and arches.

Features:

  • Effective temperature range up to 1800°F
  • Highly efficient insulation
  • Used to reduce radiation loss and air infiltration
  • Applications:

  • Roof/curved surfaces
  • End and side walls
  • Information provided by Thermal Ceramics

    Available Properties
    • Specific Heat Capacity
    • Thermal Conductivity
    • Maximum Service Temperature, Air
    • Cr2O3 content
    • Mn2O3 content
    • TiO2 content
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。