Thermal Ceramics HT Kaofil Pumpable

 

Material Notes:
Kaofil Pumpables are a mixture of Kaowool ceramic fibers and fillers dispersed in a high-temperature binder. This mix produces a stable high-temperature insulation which can be placed by forced pumping such as through a Kaowool Diaphragm Pump or a piston extrusion pump.

Kaofil Pumpables can be used in hot or cold repairs. These pumpables will air dry over time. However, at unit operating temperatures, the drying is rapid while still allowing time for the pumpable, under force, to seek out voids. Kaofil Pumpables offer good insulating properties, good strength and vibration resistance.

Features:

  • Hot spot repair
  • One-component pumpable
  • Ready to use
  • Good damming ability
  • Highly insulating
  • Applications:

  • Hot or cold repair to refractory backup insulation
  • Hot or cold repair of boiler insulation, sidewalls, and penthouses
  • Brick kiln crown and walls
  • Coke oven jambs and seals
  • Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Solids Content
    • Modulus of Rupture
    • Thermal Conductivity
    • Melting Point
    • Maximum Service Temperature, Air
    • Shrinkage
    • Shelf Life
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。