Thermal Ceramics Kao-Seal

 

Material Notes:

Refractory Castable Sealant: Kao-Seal is a water-based spray or brush sealant coating for both dense and lightweight castable refractory linings. This sealant retards alkali hydrolysis by developing an airtight interface membrane on the castable surface.

Kao-Seal is ready to use. Do not thin unless absolutely needed for applying. Typical coverage is 250 sf/gal. of full strength.

Ceramic Fiber Dust Suppressant: Kao-Seal is also a water-based spray sealant/dust suppressant for ceramic fiber products. This material reduces the tendency for fibers to become airborne before, during, or after a ceramic fiber product is handled or cut. Kao-Seal can effectively reduce dusting and airborne fibers during installation and during tear-out. This material does burn out at low temperatures, so it will need to be re-applied after exposure to heat (212°F).

Kao-Seal can be diluted for this application (up to 25% Kao-Seal to 75% water). Before using, mix by stirring or shaking. When stirring do not use sticks or paddles which could splinter or otherwise contaminate the product.

Adhesive: Kao-Seal is also a water-based adhesive which can be brushed or sprayed to adhere ceramic fiber products to a variety of surfaces including another ceramic product, a carbon steel furnace shell, stainless or aluminum foils, and textile products. Kao-Seal becomes ineffective after exposure to temperatures in excess of 212°F. As an adhesive, it is intended to be a process aid and help hold material in place until a mechanical closure or seal can be applied or other higher temperature adhesives can be applied.

Features:

  • Refractory castable sealant to retard alkali hydrolysis
  • Spray sealant/dust suppressant for ceramic fiber
  • Adhesive for ceramic fiber
  • Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Solids Content
    • Viscosity
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。