Thermal Ceramics 607 Max HM 12 Superwool Bulk
Material Notes: Superwool is uniquely designed from pure raw materials and specially processed to offer excellent performance in high temperature applications. Superwool offers an alternative to traditional solutions due to its exceptional properties of high refractoriness and excellent non-wetting characteristics in applications requiring direct contact with molten aluminum.Superwool provides stability and resistance to chemical attack. Exceptions include hydrofluoric acid, phosphoric acid and strong alkalies (i.e. NaOH, KOH). Superwool is unaffected by incidental spills of oil or water. Thermal and physical properties are restored after drying. Although Superwool’s basic fiber form offers an economical alternative for most applications, they can be engineered to meet the requirements of your most demanding application. Fiber diameter, shot content, fiber length and form can be altered as required to achieve desired properties for specific applications. Features: Low biopersistence Thermal stability Low heat storage Good resistance to tearing Flexible and resilient Immune to thermal shock Excellent thermal insulating performance Based on patented technologyApplications Expansion joints construction Base seals Low mass kiln car construction Tube seal fabrication Thermal and acoustical insulation As primary raw material for high temperature converted and engineering fibers - Enfil®Information provided by Thermal Ceramics
| Available Properties |
- Bulk Density
- Melting Point
- Maximum Service Temperature, Air
- Alumina Content
- Fiber Length, cm
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|