Thermal Ceramics 607 Superwool Pyro-Fold and Pyro-Stack Modules

 

Material Notes:
Superwool Pyro-Fold modules are accordion fold blocks used for lining industrial furnaces.

Superwool Pyro-Stack modules are similar to the Pyro-Fold modules with the blanket cut and stacked edge-grain rather than continuously folded.

Superwool, CMS wools are uniquely designed from pure raw materials (Calcium-Magnesium-Silicate), and specially processed to offer excellent performance in high-temperature applications. Superwool offers an alternative to traditional solutions due to its unique properties of high refractoriness and excellent non-wetting characteristics to applications requiring direct contact with molten aluminum. These light weight wools are resistant to thermal shock, provide low thermal conductivity and low heat storage combined with their enhanced solubility in body fluids. Superwool modules are available in a variety of attachment systems that utilize 316 stainless steel yoke and support tubes to meet most installation needs.

Superwool provides stability and resistance to chemical attack. Exceptions include hydrofluoric acid, phosphoric acid and strong alkalies (i.e. NaOH, KOH). Superwool is unaffected by incidental spills of oil or water. Thermal and physical properties are restored after drying.

Features:

  • Accordian style construction or edge-grain
  • Choice of available attachment systems
  • Non-wetting to molten aluminum
  • Low biopersistence
  • Thermal stability
  • Low heat storage
  • Flexible and resilient
  • Immune to thermal shock
  • Excellent thermal insulating performance
  • Based on patented technology
  • Applications:

  • Homogenizing furnaces
  • Process heaters
  • Ceramic kiln
  • Annealing furnace
  • Heat treating furnace
  • Thermal oxidizers
  • Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Thermal Conductivity
    • Melting Point
    • Maximum Service Temperature, Air
    • Alumina Content
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。