Thermal Ceramics 607 Blanket AC2 Superwool

 

Material Notes:
Superwool 607 Blanket AC2 is made specifically for sound absorption applications. It has excellent sound absorption characteristics, thermal stability, superior mechanical strength and vibration resistance. This product combines excellent uniformity with enhanced thermal and acoustical performance. It is flexible, easy to cut, shape and install.

Superwool 607 Blanket AC2 is made of long fibers, needled from both sides, and possesses high strength before and after heating.

Features:

  • Low biopersistence
  • Excellent sound absorption
  • Thermal stability
  • Low heat storage
  • Good resistance to tearing
  • Flexible and resilient
  • Immune to thermal shock
  • Excellent thermal insulating performance
  • Exonerated under Nota Q of Directive 97/69/EC
  • Not subject to any use restrictions under German hazardous substance regulation
  • Based on patented technology
  • Applications:

  • HRSG silencers
  • Mufflers
  • Sound Walls
  • Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Thermal Conductivity
    • Shrinkage
    • Airflow Resistance, Rayls/m
    • Leachable chlorides, ppm
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。