Thermal Ceramics 607 Blanket AC2 Superwool
Material Notes: Superwool 607 Blanket AC2 is made specifically for sound absorption applications. It has excellent sound absorption characteristics, thermal stability, superior mechanical strength and vibration resistance. This product combines excellent uniformity with enhanced thermal and acoustical
performance. It is flexible, easy to cut, shape and install. Superwool 607 Blanket AC2 is made of long fibers, needled from both sides, and possesses high strength before and after heating. Features: Low biopersistence Excellent sound absorption Thermal stability Low heat storage Good resistance to tearing Flexible and resilient Immune to thermal shock Excellent thermal insulating performance Exonerated under Nota Q of Directive 97/69/EC Not subject to any use restrictions under German hazardous substance regulation Based on patented technologyApplications: HRSG silencers Mufflers Sound WallsInformation provided by Thermal Ceramics
| Available Properties |
- Density
- Thermal Conductivity
- Shrinkage
- Airflow Resistance, Rayls/m
- Leachable chlorides, ppm
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|