Thermal Ceramics Aerotech E-Mat
Material Notes: Aerotech E-Mat is a needle-punched non-woven mat consisting of 100% glass fibers. These fibers are mechanically interlocked with no added binders or adhesives.Features: Low thermal conductivity Temperature rated to 1200°F Lightweight and flexible Non-respirable E-glass fibers Non-flammable Conforms to MIL-I-24244 Non-corrosive Will not decay or sustain mold growth ASTM E 84; 0 flame spread; 0 smoke generated No added binders or adhesives Fibers are mechanically interlocked Retains integrity upon heatingApplications: Thermal/acoustical insulation for aircraft and jet engines Highly effective thermal and acoustical insulation is required in a medium-temperature rangeInformation provided by Thermal Ceramics
| Available Properties |
- Density
- Dielectric Constant
- Dielectric Strength
- Thermal Conductivity
- Creep
- Moisture Absorbency, %
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|
|
 |
 |
请读关于材料数据的和我们的。询问或评论有关 MatWeb? 请与 联系。我们感谢您对 MatWeb的参与。
本站点由 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。
|
 |
|