Thermal Ceramics Twisted and Braided Rope Kao-Tex 1000

 

Material Notes:
Kao-Tex 1000 textile products are made from a highly textured form of silica and are coated on one side with a proprietary treatment. They are especially designed and developed for temperatures up to 1000°F (538°C).

Kao-Tex 1000 textile products have properties which include excellent tensile strength, outstanding abrasion resistance and low thermal conductivity.

The cloth has excellent seam strength for sewing and handling which is required for the fabrication of items such as gloves and mittens.

The rope is available in two different constructions – twisted and braided.

Kao-Tex 1000 textile products have improved performance over asbestos textiles in five main areas: softer hand and feel, better thermal insulating properties than asbestos material of the same weight, better dimensional stability, abrasion resistance, and strength. These advantages result from the interaction of three factors: the use of highly textured yarn, the density of the weave, and the coated surface treatment.

Applications:

  • Welding curtains
  • Fire curtains
  • Oven curtains
  • Drop curtains
  • Stress relieving blankets
  • Welding blankets
  • Safety blankets
  • Thermal insulation blankets
  • Expansion joints
  • Piping insulation
  • Electrical insulation
  • Gas and liquid filtration
  • Laminates
  • Gaskets and seals
  • Safety garments
  • Gloves and mittens
  • Aprons
  • Spats
  • Sleeves
  • Cable and wire insulation (thermal and/or electrical)
  • Hose insulation
  • Fuel line insulation
  • Door and oven gasketin.
  • Woodburning stove seals
  • Features:

  • Both forms make excellent seals or packing for temperatures lower than 1000°F (538°C)
  • Kao-Tex 1000 provides all the protection but none of the health hazards of asbestos
  • Information provided by Thermal Ceramics

    Available Properties
    • Specific Gravity
    • Melting Point
    • Maximum Service Temperature, Air
    • Fiber Length, cm
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。