Thermal Ceramics Square and Round Braided Kao-Tex 2000
Material Notes: Kao-Tex 2000 textiles are made from alumina-silica ceramic fibers that are reinforced with an organic carrier fiber for added strength and stability, making them an excellent choice for industrial applications. The nature of the engineered yarns and weave types, provide excellent strength, resulting in a physically resilient material well suited to high temperature industrial applications. Kao-Tex 2000 Textile contains 20% organic carriers that burn out at approximately 400°F causing some smoking and outgassing. Additionally, a fiberglass continuous filament is contained in the yarn for improved handbility during installation and lower temperatures. This material will degrade at 1200°F. Kao-Tex textiles exhibit excellent chemical stability resisting attack from most corrosive agents. Exceptions are hydrofluoric and phosphorous acids and concentrated alkalies. Kao-Tex textiles also resist oxidation and reduction. Features: Made from alumina-silica ceramic fiber Asbestos free High temperature use up to 2000°F Excellent chemical stability Excellent thermal shock and corrosion resistance Applications: Gaskets Seals Furnace and welding curtains Pipe wrapping Expansion joint packagingInformation provided by Thermal Ceramics
| Available Properties |
- Loss On Ignition
- Melting Point
- Maximum Service Temperature, Air
- Shrinkage
- B2O3 Content
- CaO content
- MgO Content
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|