|   TIMCAL TIMREX® KC44 Primary Synthetic Graphite  Subcategory: Graphite; Carbon; Additive/Filler for Polymer Key Words: CAS Number 7782-42-5 Material Notes: TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all production and processing stages, strict final inspection, and clearly defined development processes.
 TIMREX Primary Synthetic Graphite shows unique properties thanks to the combination of a consistent purity, perfect crystalline structure and well defined texture. Information provided by TIMCAL 
| | 
    | Available Properties |  
    | DensityParticle SizeSpecific Surface AreaAshMoisture ContentAspectCrystallinity, Lc, nmInterlayer Distance, nm
 | 
 | 
 |  | | 
    | Property Data |  
    | 