TIMCAL TIMREX® 80X150 mesh FR Natural Flake Graphite
Subcategory: Graphite; Carbon; Additive/Filler for Polymer
Key Words: CAS Number 7782-42-5
Material Notes: TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-des-Îles, Quebec, Canada. Further processing can be done either in Lac-des-Îles or for high added value products (e.g. TIMREX PG25) in our new processing plant in Terrebonne, Quebec, Canada. All TIMREX“Naturals” are thoroughly controlled in our laboratories to ensure quality, consistency and total customer satisfaction. Information provided by TIMCAL
| Available Properties |
- Bulk Density
- Particle Size
- Ash
- Moisture Content
- Aspect
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|