TIMCAL TIMREX® LSG10 Natural Graphite

 

Subcategory: Graphite; Carbon; Additive/Filler for Polymer

Key Words: CAS Number 7782-42-5

Material Notes:
TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-des-Îles, Quebec, Canada. Further processing can be done either in Lac-des-Îles or for high added value products (e.g. TIMREX PG25) in our new processing plant in Terrebonne, Quebec, Canada. All TIMREX

“Naturals” are thoroughly controlled in our laboratories to ensure quality, consistency and total customer satisfaction.

Information provided by TIMCAL

Available Properties
  • Density
  • Particle Size
  • Ash
  • Moisture Content
  • Aspect
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。