TIMCAL TIMREX® LB1300 Aqueous Dispersion
Subcategory: Graphite; Carbon; Additive/Filler for Polymer
Material Notes: TIMREX® LB 1300 is a stable binder free aqueous dispersion of graphite powder. It serves as a versatile base product for the formulation of dispersions by adding suitable binders.Information provided by TIMCAL
| Available Properties |
- Density
- Solids Content
- Particle Size
- pH
- Ash
|
|
|
|