CoorsTek Dura-Z™ MgO Partially Stabilized Zirconia
Subcategory: Oxide, Zirconium; Oxide
Key Words: ZrO2
Material Notes: Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a sharp decrease in the flexural strength of the sample. Data Provided by the manufacturer, CoorsTek, Inc.
| Available Properties |
- Density
- Water Absorption
- Particle Size
- Knoop Microhardness
- Hardness, Rockwell 45 N
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Strength
- Compressive Strength
- Poissons Ratio
- Fracture Toughness
- Shear Modulus
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|