Zircar Zirconia ZR-CEM Zirconia Cement

 

Subcategory: Oxide, Zirconium; Oxide

Key Words: ZrO2, zirconium oxide

Material Notes:
Zircar Zirconia Cement Type ZR-CEM is an off white single part yttria-stabilized zirconia adhesive with a useful temperature limit of 2200°C. ZR CEM is formulated specifically for bonding Zircar Zirconia Felts, Boards and Cylinders to themselves or to back-up thermal insulations such as porous firebrick, alumina fiber and alumino-silicate fiber boards. ZRCEM is composed of yttria-stabilized zirconia milled fibers and sub-micron particles. Potassium silicate and zirconium acetate binders are added to enhance bonding characteristics. ZR-CEM will not bond to non-porous surfaces such as glass or steel. ZR-CEM is mildly acidic (pH 5.4) and forms a strong bond upon removal of the water solvent.

For most furnace applications, the articles bonded together are ready for placing in service once the cement has dried. Curing at 426°C (800°F) or more may be desirable to eliminate the acetate prior to use. The cured bond joint is stronger than the tensile strength of 30 pound per cubic foot density Zircar Zirconia insulation material Types ZYFB-3, ZYZ-3 and ZYC. Pull out or de-lamination due to excessive mechanical or thermal stresses will usually first occur in the insulation material itself.

ZR-CEM has the consistency of a thick paint and should be mixed thoroughly before using. ZR-CEM may be applied by dipping, brushing, or rolling. If ZR-CEM becomes thickened by evaporation, de-ionized or distilled water can be used to bring the cement back to its original consistency. ZR-CEM is non-flammable and is not affected by freezing. For a 0.01 inch thick bond, a pint of cement will cover about 7 square feet of joint surface.

Features:

  • High Temperature Stability to 2200°C
  • Withstands Water and Steam after curing
  • Safe to Use – Non-Flammable
  • Excellent Thermal Shock Resistance
  • Low Shrinkage, High Strength
  • Available ‘Off the Shelf’
  • Single Part System

Information provided by Zircar Zirconia.

Available Properties
  • Bulk Density
  • Solids Content
  • Viscosity
  • Melting Point
  • Maximum Service Temperature, Air
  • Trace Inorganics
  • Weight Per Pint
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。