Zircar Zirconia ZHB Zirconia Hollow Balls

 

Subcategory: Oxide, Zirconium; Oxide

Key Words: ZrO2, zirconium oxide

Material Notes:
Zirconia Hollow Balls Type ZHB are sintered calcia-stabilized zirconia hollow balls, which flow easily into a confined space. Our standard product is our Type ZHB-1 which ranges in particle size from 0.2 mm to 3.0 mm diameter, which fill space effectively. They are useful for high temperature insulation in spaces where the insulation must be poured into place. The different size balls tend to segregate when poured as the larger balls tend to ‘float’ on top of the smaller balls. To minimize this effect, pour all the balls in at one time.

Application Information:

Zirconia Hollow Balls Type ZHB are useful as heat exchange media in fluidized bed reactors and as insulation in constrained spaces in very high temperature applications. The melting point of ZHB exceeds 4000°F. ZHB can be sieved into a more narrow size distribution on request.

Information provided by Zircar Zirconia.

Available Properties
  • Specific Gravity
  • Bulk Density
  • Angle of Repose
  • Color
  • Crystal Structure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。