Zircar Zirconia ZYF-A2.13 Zirconia Felt
Subcategory: Oxide, Zirconium; Oxide
Key Words: ZrO2, zirconium oxide
Material Notes: Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains its fibrous nature to 2480°C. The stabilized zirconia composition permits the advantages of fibrous insulations to be extended into temperature regions well above the melting temperatures of siliceous and alumina insulation materials. Zirconia Felt Type ZYF-A2.13 is ZYF-150 in which the zirconia fibers have been surface treated with colloidal alumina, refired, and face milled to provide a very uniform thickness. This post processing results in a stiff sheet. Features: - Low Thermal Conductivity
- High Porosity
- High Purity
- Extreme High Temperature Stability
- Fibers Stabilized with ~10 wt% Yttria
- Custom Fillers and Coatings Available
- Can be Cemented with Zircar Zirconia Cement Type ZR-CEM
- Can be Rigidized with Zircar Zirconia Rigidizer Type ZIR-RIG
- Easily Cut to Size
- Available “Off the Shelf”
Application Information: - This thicker, rigidized felt was developed for use as a diffusion burner membrane for fuel fired heaters installed in long-haul trucks and high end passenger cars. In this application the liquid fuel, gasoline or diesel, is pumped onto one surface of a disk of felt. The fuel then wicks through to the opposite surface which is located in a combustion chamber and evaporates. The evaporated fuel is mixed with air and ignited providing an ‘instant-on’ heat in the vehicle which is independent of the engine heat.
- ZYF-A2.13 is also used as a setter plate for vacuum sintering flat sheets of powdered metal materials. The felt remains flat during sintering because of its rigid structure.
Information provided by Zircar Zirconia.
Available Properties |
- Bulk Density
- Porosity
- Thickness
- Compressive Strength
- Shrinkage
- Tensile Strength per Unit Width
- Weight Per Area
- Wrapping Diameter Before Breaking
|
|
|
|
Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|