Zircar Zirconia ZYW-30A Zirconia Cloth

 

Subcategory: Oxide, Zirconium; Oxide

Key Words: ZrO2, zirconium oxide

Material Notes:
Zirconia Cloths Type ZYW are flexible textiles composed of yttria stabilized zirconia fibers that offer extreme temperature and chemical resistance in a flexible form. Type ZYW cloths provide the lowest thermal conductivity of any commercially available refractory material in their class. Type ZYW cloths are true textiles, manufactured using the Zircar process where an organic cloth is converted into an inorganic replica. The fabrics are constructed of continuous individual filaments mechanically interlocked in a woven structure.

ZYW ceramic textiles are ideal for temperatures up to 2200°C and are suitable for applications such as high energy battery separators, thermal insulation in crystal growing furnaces, and hot gas filtration. The fine capillary and pore structure of ZYW, in combination with the hydrophilic nature of zirconia, impart excellent wetting, solution retention, and wicking characteristics, to these materials. The cloths require neither binders nor supporting wires to maintain their construction and will comply somewhat to both tensile and compressive forces due to the mechanical interlocking of the fibers. Elongation of 4 to 8% before breaking allows ZYW to conform to irregular surfaces. ZYW can be compressed up to two-thirds of its normal thickness and still recover a major fraction of its original dimension with little fiber damage.

Zirconia Cloth Type ZYW is available in two formats; Type ZYW-15 and Type ZYW-30A. Type ZYW-15 is a square weave cloth nominally 0.015” thick composed of yttria-stabilized zirconia fibers. Type ZYW-30A is a satin weave cloth nominally 0.025” thick.

Features:

  • Low Thermal Conductivity
  • High Porosity
  • Offered in Two Constructions: Square Weave and Satin Weave
  • Extreme High Temperature Stability
  • Fibers Stabilized with ~10 wt% Yttria
  • Can be Cemented with Zircar Zirconia Cement Type ZR-CEM
  • Can be Rigidized with Zircar Zirconia Rigidizer Type ZR-RIG
  • Easily Cut to Size
  • Available ‘off the shelf’

Information provided by Zircar Zirconia.

Available Properties
  • Bulk Density
  • Porosity
  • Thickness
  • Vapor Pressure
  • Specific Heat Capacity
  • Melting Point
  • Maximum Service Temperature, Air
  • Shrinkage
  • Tensile Strength per Unit Width
  • Weight Per Area
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。