Zircar Zirconia YK-15 Yttria Knit Textile

 

Subcategory: Oxide, Other; Oxide

Key Words: Y2O3, yttrium oxide

Material Notes:
Yttria (yttrium oxide - Y2O3) is typically used as a stabilizer for zirconia. It is offered here in its pure and stable metal oxide form, which is not attacked by most molten metals, including lithium and titanium. Our high purity yttria fiber and textiles are offered in six different standard product forms; bulk fiber Type YBF, two felts Types YF-50 and YF-100 and three types of knit cloth Types YK-15, YW-15 and YW-30.

Features:

  • High Purity
  • High Temperature Stability
  • Low Thermal Conductivity
  • Excellent Thermal Shock Resistance
  • No Outgassing
  • Six Different Product Formats Offered
  • Available ‘Off the Shelf’

Application Information:

  • Yttria textiles are used in the development of large grain Rare Earth Barium Copper Oxide (REBCO) melt processed high temperature superconductors (HTS).

Information provided by Zircar Zirconia.

Available Properties
  • Bulk Density
  • Loss On Ignition
  • Porosity
  • Outgassing - Total Mass Loss
  • Melting Point
  • Shrinkage
  • Tensile Strength per Unit Width
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。