Zircar Zirconia Buster M-35 Alumina Boards, Discs, and Cylinders
Subcategory: Oxide, Zirconium; Oxide
Key Words: Al2O3, aluminum oxide
Material Notes: Zircar alumina insulation Type Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with either a high purity alumina binder in BusterA-30 for use at 1600C or with silica binders in BusterM-35 that form a more thermal shock resistant mullite bond for use at 1700C. Both types of Buster boards are pre-fired for organic-free use. Their fine grain quality enables precision machining. All these features make Buster an ideal insulation material for hot face insulation in both industrial furnaces and thermal process systems. Buster is available in boards, cylinders and custom machined parts. Features: - 1600°C & 1700°C Rated Versions
- Alumina or Mullite Bonded
- High Strength
- Low Thermal Conductivity
- 100% Fibers & Binder - No Fillers
- Excellent Machinability
- Non-RCF Composition
Information provided by Zircar Zirconia.
| Available Properties |
- Specific Gravity
- Porosity
- Tensile Strength @ Break
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity at Elevated Temperature
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|