Zircar Zirconia Buster Alumina Mat

 

Subcategory: Oxide, Zirconium; Oxide

Key Words: Al2O3, aluminum oxide

Material Notes:
Buster Blanket and Buster Mat are flexible, Hi-Alpha alumina fiber insulation materials. The mat is 100% fibers while the blanket has been needled into a durable blanket with the addition of an organic fiber reinforcement. Both forms have useful properties up to 1600°C. These polycrystalline fiber blankets offer higher temperature capability, less shrinkage and greater chemical resistance than standard alumina-silica blankets. Buster Mat exhibits lower thermal conductivity, lower thermal mass and greater thermal shock resistance than all alumina-silica blankets, while also providing a much cleaner insulation. The minor addition of silica modifies the alumina fiber's microcrystalline structure and acts as a grain growth inhibitor and prevents embrittlement that usually occurs in pure alumina after extended use at elevated temperatures. Buster Mat resists attack in aggressive chemical environments due to its high purity & refractory nature. It is stable in vacuum, inert, oxidizing or reducing atmospheres. Flexible Buster products are useful as insulation packing in furnace spaces, around furnace sight tubes & ports and as filler in expansion joints and masonry cracks.

Features:

  • Available in Two Different Forms
  • Low Thermal Conductivity
  • Highly Refractory
  • Non-RCF Fibers
  • Low Shrinkage up to 1500°C
  • 97% Pure Alumina
  • Available “Off the Shelf”

Information provided by Zircar Zirconia.

Available Properties
  • Bulk Density
  • Thermal Conductivity at Elevated Temperature
  • Melting Point
  • Maximum Service Temperature, Air
  • Shrinkage
  • Trace Impurities
  • Trace Inorganics
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。