ZIRCAR Ceramics Castertip Type-ASQ
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes: 14 pcf density refractory ceramic fiber "soft tip". Alumina bonding of shot free fiber results in extreme performance in manufacture of the finest grades of medical, food and packaging foils. Information provided by Zircar Ceramics.