ZIRCAR Ceramics Castertip Type Z-290
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes: 29 pcf density refractory ceramic fiber "medium tip". Silica bonded shot-free fiber and fillers impart great mechanical strength. Z-290 works to help SCAL operators run their machines faster and longer. Information provided by Zircar Ceramics.
| Available Properties |
- Density
- Loss On Ignition
- Specific Surface Area
- Hardness, Shore A
- Modulus of Rupture
- Compressive Strength
- Shrinkage
|
|
|
|
| Property Data |