ZIRCAR Ceramics Alumina Rigidizer/Hardener Type AL-R/H
Subcategory: Oxide, Aluminum; Ceramic/Metallic Coating; Oxide
Material Notes: Type AL-R/H Alumina Rigidizer/Hardener is a single part water based colloidal suspension of alumina hydrate. Mainly used for rigidizing and hardening the surfaces of ZIRCAR® fibrous ceramic products it also finds use as a coating agent and binder. Information provided by Zircar Ceramics.
| Available Properties |
- Density
- pH
- Specific Surface Area
- Melting Point
- Maximum Service Temperature, Air
- Alumina Content of Liquid
- Alumina Purity
- Color
- Weight per gallon
|
|
|
|