ZIRCAR Ceramics Alumina-Silica Cement Type AS-CEM
Subcategory: Oxide, Silicon; Oxide, Aluminum; Ceramic/Metallic Coating; Oxide
Material Notes: Type AS-CEM Alumina-Silica Cement is a high temperature resistant cement useful for creating a hard coating on the surfaces of ZIRCAR® Alumina-Slica fibrous ceramic products or other porous insulating Materials. It has useful properties to 1260°C (2300°F). Information provided by Zircar Ceramics.
| Available Properties |
- Dielectric Strength
- CTE, linear 68°F
- Maximum Service Temperature, Air
- Shrinkage
- Color
|
|
|
|