ZIRCAR Ceramics Alumina Papers Type APA-1
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes: Flexible and rigid grades of high alumina fiber paper in sheets, full rolls and die cut parts. They are useful to temperatures as high as 1650°C (3002°F). Information provided by Zircar Ceramics.
| Available Properties |
- Density
- Thickness
- Tear Strength
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Color
- Form
- Organics
- Type of Binder
- Weight
|
|
|
|
| Property Data |