ZIRCAR Ceramics Alumina Mat
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes: A layered, low density flexible mat made of 100% polycrystalline alumina fiber (non-RCF) designed for use to temperatures as high as 1650°C (3002°F). Shot free low density mat used as fill between rigid insulation materials as well as a source for making folded fiber modules. Information provided by Zircar Ceramics.
| Available Properties |
- Density
- Loss On Ignition
- Filament Diameter
- Thickness
- Hardness, Mohs
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Specific Heat Capacity
- Thermal Conductivity at Elevated Temperature
- Melting Point
- Maximum Service Temperature, Air
- Shrinkage
- Color
- Shot Content
|
|
|
|