ZIRCAR Ceramics ZIRPORCOAT Hydrophilic Inorganic Coating
Subcategory: Ceramic/Metallic Coating
Material Notes: ZIRPORCOAT is a single-part hydrophilic inorganic coating designed specifically for use with MICROSIL Microporous Insulation. It consists of silicates and an inorganic binder and after application has useful properties to 900°C (1652°F). Applied by brushing or dipping ZIRPORCOAT combines with the surface of the MICROSIL and works to increase its surface hardness. It also improves edge stability, handleability and reduces particulate generation. Information provided by Zircar Ceramics.
|
|
|