ZIRCAR Ceramics Alumina Insulation Type SALI Moldable
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes: A close cousin to premium grade Type SALI insulation, SALI Moldable is a thick doughy material readily shaped into complex forms using molds & hand building techniques or applied to surfaces. When dried and fired, parts made of it are useful to 1700°C (3092°F). Information provided by Zircar Ceramics.
| Available Properties |
- Density
- Bulk Density
- Solids Content
- pH
- Melting Point
- Maximum Service Temperature, Air
- Shrinkage
- Color
|
|
|
|