ZIRCAR Ceramics Alumina Bubble Type IB-100B
Subcategory: Oxide, Aluminum; Oxide
Material Notes: Thin wall aluminum oxide ceramic spheres offered in 2 standard bubble sizes. These low density sintered ceramic bodies are useful in a range of refractory applications with temperatures to 2000°C (3632°F). Information provided by Zircar Ceramics.
|
|
|
| Property Data |