ZIRCAR Ceramics Alumina Refractory Castable Type ZIRALCAST 95
Subcategory: Oxide, Aluminum; Oxide
Material Notes: Hydraulically setting castable refractory containing high purity fused alumina "bubbles". This low density castable can be used like concrete and produces ceramic bodies useful in a range of applications with temperatures to 1800°C (3272°F). Information provided by Zircar Ceramics.
| Available Properties |
- Density
- Particle Size
- Modulus of Rupture
- Modulus of Rupture
- Thermal Conductivity at Elevated Temperature
- Shrinkage
- Dry Time
- Water of Hydration
|
|
|
|