ZIRCAR Ceramics Alumina Insulation Type SALI
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes: SALI has been serving 1700°C low mass furnace users longer than any other alumina fiber board available today. SALI is a premium grade rigid fiber board with superior hot strength. Information provided by Zircar Ceramics.
| Available Properties |
- Density
- Open Porosity
- Flexural Strength
- Compressive Strength
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity at Elevated Temperature
- Melting Point
- Maximum Service Temperature, Air
- Softening Point
- Shrinkage
- Bond
- Color
|
|
|
|