ZIRCAR Ceramics Alumina Insulation Type ALCAA
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes: ALC is the same material as ZAL-15 - but brings exceptional uniformity in an insulation material in cylindrical form. Information provided by Zircar Ceramics.
| Available Properties |
- Density
- Open Porosity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity at Elevated Temperature
- Melting Point
- Maximum Service Temperature, Air
- Shrinkage
- Bond
- Color
|
|
|
|