Zircar Refractory Composites Alumina-Silica Fiber Paper ASPA-1

 

Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide

Material Notes:
ASPA-1 is a premium grade, lightweight refractory material made from high purity alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal conductivity and is designed for use in applications where purity, cracking resistance, high strength and resistance to heat are paramount. Due to its exceptional resistance to heat flow for its thickness, it provides maximum thermal resistance where space is at a premium. This material is virtually shot free and is the cleanest refractory paper available. It is ideal for applications up to 1260°C (2300°F). Type ASPA-1 contains an organic binder to provide increased handling strength at room temperature. It possesses excellent chemical stability and resists attack from most corrosive agents. Because of its high purity chemistry, it resists oxidation and reduction. If it becomes wet due to water, steam or oil, its physical and thermal properties will return upon drying.

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Available Properties
  • Density
  • Loss On Ignition
  • Dielectric Strength
  • Thermal Conductivity at Elevated Temperature
  • Melting Point
  • Maximum Service Temperature, Air
  • Color
  • Fiber Index, %
  • Mullen Burst, psi
  • Tensile Strength, g/in
  • Type of Binder
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。