Zircar Refractory Composites Alumina-Silica Fiber Paper ASPA-880

 

Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide

Material Notes:
ASPA-880 is a high temperature, lightweight refractory material made from alumina-silica fibers formed into highly flexible sheets. It is made from shorter and smaller diameter fibers with a higher alumina content and are laid up at significantly higher density. These factors lead to high temperature, slow shrinkage, higher strength, and better chemical resistivity. This alumina-silica fiber paper exhibit very low thermal conductivity and is designed for use in applications where flexibility, high strength and resistance to heat are paramount. Type ASPA-880 exhibits low thermal conductivity and is ideal for applications up to 1450°C (2642°F). It is used in environments where standard ceramic fiber papers will not survive.

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Available Properties
  • Density
  • Loss On Ignition
  • Thermal Conductivity at Elevated Temperature
  • Melting Point
  • Maximum Service Temperature, Air
  • Color
  • Fiber Index, %
  • Mullen Burst, psi
  • Tensile Strength, g/in
  • Type of Binder
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。