Zircar Refractory Composites Alumina-Silica Fiber Paper ASPA-880
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes: ASPA-880 is a high temperature, lightweight refractory material made from alumina-silica fibers formed into highly flexible sheets. It is made from shorter and smaller diameter fibers with a higher alumina content and are laid up at significantly higher density. These factors lead to high temperature, slow shrinkage, higher strength, and better chemical resistivity. This alumina-silica fiber paper exhibit very low thermal conductivity and is designed for use in applications where flexibility, high strength and resistance to heat are paramount. Type ASPA-880 exhibits low thermal conductivity and is ideal for applications up to 1450°C (2642°F). It is used in environments where standard ceramic fiber papers will not survive.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)
| Available Properties |
- Density
- Loss On Ignition
- Thermal Conductivity at Elevated Temperature
- Melting Point
- Maximum Service Temperature, Air
- Color
- Fiber Index, %
- Mullen Burst, psi
- Tensile Strength, g/in
- Type of Binder
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|